Crystal Structure and Surface Analysis of Diamond-Like Semiconductor Single Crystals

Publication Information:

Rosmus, K., J. Brant, J. Sturgeon, K. Bunker, K. Harris, J. Aitken, Crystal Structure and Surface Analysis of Diamond-Like Semiconductor Single Crystals, MS&T 2011, Columbus, OH, October 16-20, 2011 (Platform Presentation).

Year: 2011